000 | 04076nam a22005295i 4500 | ||
---|---|---|---|
001 | 978-94-017-7252-5 | ||
003 | DE-He213 | ||
005 | 20200421111204.0 | ||
007 | cr nn 008mamaa | ||
008 | 150930s2016 ne | s |||| 0|eng d | ||
020 |
_a9789401772525 _9978-94-017-7252-5 |
||
024 | 7 |
_a10.1007/978-94-017-7252-5 _2doi |
|
050 | 4 | _aTA401-492 | |
072 | 7 |
_aTNK _2bicssc |
|
072 | 7 |
_aTEC009020 _2bisacsh |
|
072 | 7 |
_aTEC021000 _2bisacsh |
|
082 | 0 | 4 |
_a691 _223 |
245 | 1 | 0 |
_aRILEM Recommendations for the Prevention of Damage by Alkali-Aggregate Reactions in New Concrete Structures _h[electronic resource] : _bState-of-the-Art Report of the RILEM Technical Committee 219-ACS / _cedited by Philip J. Nixon, Ian Sims. |
250 | _a1st ed. 2016. | ||
264 | 1 |
_aDordrecht : _bSpringer Netherlands : _bImprint: Springer, _c2016. |
|
300 |
_aXVI, 168 p. 20 illus. _bonline resource. |
||
336 |
_atext _btxt _2rdacontent |
||
337 |
_acomputer _bc _2rdamedia |
||
338 |
_aonline resource _bcr _2rdacarrier |
||
347 |
_atext file _bPDF _2rda |
||
490 | 1 |
_aRILEM State-of-the-Art Reports, _x2213-204X ; _v17 |
|
505 | 0 | _aIntroduction, by Philip J Nixon & Ian Sims -- RILEM Recommended Test Method: AAR-0, Outline Guide to the Use of RILEM Methods in the Assessment of the Alkali-Reactivity Potential of Aggregates -- RILEM Recommended Test Method: AAR-1.1, Detection of potential alkali-reactivity, Part 1: Petrographic Examination Method -- RILEM Recommended Test Method: AAR-2, Detection of potential alkali-reactivity, Accelerated Mortar-bar Test Method for Aggregates -- RILEM Recommended Test Method: AAR-3, Detection of potential alkali-reactivity, 38�C Test Method for Aggregate Combinations using Concrete Prisms -- RILEM Recommended Test Method: AAR-4.1, Detection of potential alkali-reactivity, 60�C Test Method for Aggregate Combinations using Concrete Prisms -- RILEM Recommended Test Method: AAR-5, Detection of potential alkali-reactivity, Rapid Preliminary Screening Test for Carbonate Aggregates -- RILEM Recommended Specification: AAR-7.1, International Specification to Minimise Damage from Alkali Reactions in Concrete, Part 1: Alkali-Silica Reaction -- RILEM Recommended Specification: AAR-7.2, International Specification to Minimise Damage from Alkali Reactions in Concrete, Part 2: Alkali-Carbonate Reaction -- RILEM Recommended Specification: AAR-7.3, Preliminary International Specification to Minimise Damage from Alkali Reactions in Concrete, Part 3: Concrete Dams and Other Hydro Structures. | |
520 | _aThis book contains the full set of RILEM Recommendations which have been produced to enable engineers, specifiers and testing houses to design and produce concrete which will not suffer damage arising from alkali reactions in the concrete. There are five recommended test methods for aggregates (designated AAR-1 to AAR-5), and an overall recommendation which describes how these should be used to enable a comprehensive aggregate assessment (AAR-0). Additionally, there are two Recommended International Specifications for concrete (AAR-7.1 & 7.2) and a Preliminary International Specification for dams and other hydro structures (AAR-7.3), which describe how the aggregate assessment can be combined with other measures in the design of the concrete to produce a concrete with a minimised risk of developing damage from alkali-aggregate reactions. | ||
650 | 0 | _aEngineering. | |
650 | 0 | _aGeochemistry. | |
650 | 0 | _aBuilding materials. | |
650 | 0 | _aStructural materials. | |
650 | 1 | 4 | _aEngineering. |
650 | 2 | 4 | _aBuilding Materials. |
650 | 2 | 4 | _aStructural Materials. |
650 | 2 | 4 | _aGeochemistry. |
700 | 1 |
_aNixon, Philip J. _eeditor. |
|
700 | 1 |
_aSims, Ian. _eeditor. |
|
710 | 2 | _aSpringerLink (Online service) | |
773 | 0 | _tSpringer eBooks | |
776 | 0 | 8 |
_iPrinted edition: _z9789401772518 |
830 | 0 |
_aRILEM State-of-the-Art Reports, _x2213-204X ; _v17 |
|
856 | 4 | 0 | _uhttp://dx.doi.org/10.1007/978-94-017-7252-5 |
912 | _aZDB-2-ENG | ||
942 | _cEBK | ||
999 |
_c54004 _d54004 |